Alloy Digest (1988) 37 (3): Cu-536.
Published: 01 March 1988
... UNS NO. C36000 is a leaded brass suitable for high-speed screw-machine work. It has many uses such as hardware, gears and pinions. Its trade names include free-turning brass, free-cutting yellow brass and high-leaded brass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2021) 70 (3): Cu-918.
Published: 01 March 2021
... Mueller Brass C36000 is a wrought, Cu-Zn-Pb alloy (leaded brass) that is suitable for high-speed screw machining applications and moderate thread rolling. On the basis of strength alone, it can safely be substituted for leaded steel in many applications. UNS C36000 is the most important commercial...
Journal Articles
Alloy Digest (2011) 60 (4): Cu-797.
Published: 01 April 2011
... International® 2011 2011 ASM International ANSONIA ALLOY C36000 chemical composition elasticity hardness heat treatability joinability machinability physical properties tensile properties workability thermal properties UNS C36000 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2011, ASM...
Journal Articles
Alloy Digest (1989) 38 (7): Cu-548.
Published: 01 July 1989
... International® 1996 1996 ASM International chemical composition Copper alloy no. C36000 corrosion-resistant alloys cutting tools elasticity hardness heat treatability joinability machinability physical properties shear strength tensile properties workability UNS C36000 wrrtn ALLUY NV...
Journal Articles
Alloy Digest (2001) 50 (9): Cu-672.
Published: 01 September 2001
... corrosion-resistant alloys elasticity hardness heat treatability joinability physical properties tensile properties WIELAND-Z23 workability thermal properties UNS C36000 Wieland-Z23 is a free-machining brass. The contrasting material properties of free machining and cold working...
Journal Articles
Alloy Digest (2001) 50 (2): Cu-658.
Published: 01 February 2001
... joinability physical properties SWISSMETAL SM150 SWISSMETAL SM154N SWISSMETAL SM186N workability thermal properties UNS C36000 Swissmetal alloys SM154N, 150N, and 184N, are brass alloys with high copper content and good cold forming. SWISSMETAL® SM154N, SM150, SM186N (Boillat 61A, 61T, 61D) (Free...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-820.
Published: 01 June 2013
...%. Machinability: This alloy possesses good machining characteristics. The machinability rating for C27450 is 70% of free cutting brass. This alloy is a modification of the UNS C36000 chemistry in that the missing lead is replaced with zinc. This grade is not proprietary; it is covered by industry consensus...
Journal Articles
Alloy Digest (2016) 65 (8): Cu-849.
Published: 01 August 2016
... machining characteristics. The machinability rating for C27451 is 70% of free- cutting brass. This alloy is a modification of the UNS C36000 chemistry in that the missing lead is replaced with zinc. This grade is not proprietary; it is covered by industry consensus standards. It keeps a small amount of lead...
Journal Articles
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
... welding (seam) Rating Excellent Excellent 20%(a) Excellent Excellent Good Good Not recommended Good Good (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life General Characteristics High...
Journal Articles
Alloy Digest (2020) 69 (12): Cu-908a.
Published: 01 December 2020
... welding Not recommended Coated metal arc welding Not recommended Spot welding Not recommended Seam welding Not recommended Butt welding Fair Source: Copper Development Association. (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating...
Journal Articles
Alloy Digest (2020) 69 (11): Cu-914.
Published: 01 November 2020
.... (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life equipment. Typical applications include fiber optic connectors, hardware, screws for MRI machines, sensors, sleeves, spectacle frames, spray...
Journal Articles
Alloy Digest (1982) 31 (11): Cu-447.
Published: 01 November 1982
...® 1996 1996 ASM International ANACONDA ALLOY 360 chemical composition corrosion-resistant alloys ductility elasticity hardness heat treatability joinability machinability physical properties pinions screw machine products tensile properties workability UNS C36000 I ANACONDA...
Journal Articles
Alloy Digest (2022) 71 (10): Cu-934.
Published: 01 October 2022
... Oxyacetylene welding Gas shielded arc welding Coated metal arc welding Spot welding Seam welding Rating 20% Excellent Excellent Good Excellent Not recommended Not recommended Not recommended (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating...
Journal Articles
Alloy Digest (2020) 69 (5): Cu-908.
Published: 01 May 2020
... Association. (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life. Applications Alloy C34500 is used for screw machine applications that require an alloy with the ability to be cold formed...
Journal Articles
Alloy Digest (1985) 34 (1): Cu-489.
Published: 01 January 1985
... products screws tensile properties workability UNS C36000 MUELLER Alloy 3602 Filing Code: Cu-489 Copper Alloy JANUARY 1985 - DATA ON WORLD WIDE METALS AND AlJ,OYS @I Copyright 1980. Engineering Publications, Inc. AN rights reserved. ISSN : 002-6 14X Published by Alloy Digest. Inc. 27 Canfield Street...
Journal Articles
Alloy Digest (2023) 72 (12): Cu-943.
Published: 01 December 2023
... welding Seam welding Butt welding Rating Excellent Good 40% 20%(a) Good Good Not recommended Good Good Good Fair Fair (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life ...
Journal Articles
Alloy Digest (2022) 71 (12): Cu-936.
Published: 01 December 2022
... of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life. Source: C48500, Copper Development Association Supplier Mueller Brass Company (a subsidiary of Mueller Industries Inc.) 150 Schilling Blvd. Suite 100 Collierville, Tennessee 38017, USA Tel: +1 901...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life. Source: Copper Development Association Fig. 1 Comparison of yield strength (gray bars) and electrical conductivity performance of select hard temper brass materials Supplier Wieland Rolled Products...
Journal Articles
Alloy Digest (2022) 71 (2): Cu-929.
Published: 01 February 2022
... of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life. (b) GTAW, GMAW Supplier Austral Wright Metals 133-139 Cowpasture Road Wetherill Park, New South Wales 2164, Australia Tel: +61 02 9827 0790 Web: www.australwright.com.au All data from 5% Phosphor...
Journal Articles
Alloy Digest (2020) 69 (12): Cu-915.
Published: 01 December 2020
...%(a) Excellent Excellent Fair Excellent Not recommended Source: Copper Development Association and Aurubis AG. (a) Machinability rating is expressed as a percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life. life. It may be necessary...