Skip Nav Destination
Close Modal
Search Results for
UNS C35330
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
UNS C35330
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (9): Cu-825.
Published: 01 September 2013
... workability UNS C35330 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2013, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter...
Abstract
View article
PDF
Mueller Alloy C35330 has excellent machining characteristics and resists dezincification. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Cu-825. Producer or source: Mueller Industries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (1): Cu-675.
Published: 01 January 2002
... composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties tensile properties WIELAND-Z35 workability thermal properties UNS C35330 Chemical Composition, wt (Reference Chemistry) Copper 62 Lead 2.5 Arsenic 0.1 Zinc bal Physical...
Abstract
View article
PDF
Wieland-Z35 is a medium leaded grade with a good cold-working capacity. The alloy contains arsenic and becomes dezincification resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-675. Producer or source: Wieland Metals Inc., Wieland-Werke AG.