Alloy Digest (1990) 39 (12): Cu-556.
Published: 01 December 1990
... chemical composition Copper alloy no. C32000 corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability machinability physical properties screw-machine products shear strength tensile properties workability wrought brass UNS C32000 - DIGEST- DATA...