Alloy Digest (2003) 52 (3): Cu-698.
Published: 01 March 2003
... applications chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability physical properties tensile properties WIELAND-Z20 workability thermal properties UNS C28000 Chemical Composition, wt (Reference Chemistry) Copper 61 Lead 0.2 Zinc bal Physical...
Journal Articles
Alloy Digest (1981) 30 (6): Cu-418.
Published: 01 June 1981
... composition corrosion-resistant alloys ductility elasticity hardness heat exchanger tubes heat treatability joinability machinability physical properties tensile properties workability wrought brass UNS C28000 ANACONDA Alloy 280 Filing Code: 01418 Copper Alloy JUNE 1881 - DATA ON WORLD WIDE...