Alloy Digest (2009) 58 (7): Cu-772.
Published: 01 July 2009
... composition elasticity heat treatability jewelry joinability machinability ornamental trim physical properties shear strength tensile properties workability thermal properties UNS C22600 ANSONIA ALLOY C22600 (Binary Brass Alloy) Ansonia alloy C22600 is a 12.5% Zn alloy with the previous trade...
Journal Articles
Alloy Digest (2019) 68 (2): Cu-884.
Published: 01 February 2019
... UNS CC22600 Olin Brass Alloy C22600 is a brass alloy with resistance to corrosion and has good electrical conductivity. Chemical Composition, wt.% (Nominal) Iron 0.05 max Copper 86.0 89.0 Copper plus named elements 99.8 Lead 0.05 max Zinc bal Physical Properties Electrical Conductivity. Depending...