Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
... Austral Wright Copper Alloy 220 (UNS C22000), also known as 90/10 gilding metal, is a wrought copper-zinc alloy. It combines a rich golden color with the best combination of strength, ductility, and corrosion resistance of the plain copper-zinc alloys. It weathers to a rich bronze color and can...
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
... Rolled Products NA. Producer or Source: Wieland Rolled Products NA Copyright © ASM International® 2021 2021 ASM International Wieland C22000 chemical composition physical properties tensile properties corrosion-resistant alloys workability heat treatability machinability UNS C22000...
Journal Articles
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
... composition hardness heat treatability jewelry joinability machinability ornamental trim physical properties shear strength tensile properties workability thermal properties UNS C22000 ANSONIA ALLOY C22000 (Binary Brass Alloy) Ansonia alloy C22000 is a 10% Zn alloy with the previous trade name...
Journal Articles
Alloy Digest (2002) 51 (11): Cu-692.
Published: 01 November 2002
... UNS C22000 Chemical Composition, wt Copper 90 Lead 0.05 max Iron 0.05 max Zinc bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8800 (0.318) Coefficient of linear thermal 18.2 (10.1) expansion, 10 6/K (10 6/°F) Electrical conductivity, 22 (37) 106 S/m (%IACS) Thermal conductivity, 184 (106) W/m...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-411.
Published: 01 February 1981
...-resistant alloys cosmetic containers dezincification elasticity hardness heat treatability joinability machinability munitions physical properties tensile properties workability wrought brass UNS C22000 ANACOWDA Alloy 220 Filing Code: cu411 Copper Alloy FEBRUARY 1981 - DATA ON WORLD WIDE...
Journal Articles
Alloy Digest (2008) 57 (7): Cu-756.
Published: 01 July 2008
... combines the natural corrosion resistance of C22000 with the machinability typical of leaded brasses. Like C22000, it is an alpha brass nominally composed of 89% Cu and 9% Zn, but it also contains approximately 2% lead to impart free-cutting characteristics. The relatively low zinc content of C31400...
Journal Articles
Alloy Digest (2009) 58 (7): Cu-772.
Published: 01 July 2009
... and C22000 and still as equally pleasing in color. Product Forms Available: Alloy C22600 can be supplied as wire. For other forms, contact the producer. Applications: Although this alloy is frequently referred to as jewelry bronze because of its rich color, C22600 has a wider variety of applications than...