Alloy Digest (2016) 65 (12): Cu-854.
Published: 01 December 2016
... SUPERKFC physical properties tensile properties workability thermal properties UNS C19240 Kobelco Alloy SuperKFC has high strength and high conductivity for electronic applications. The alloy is nominally Cu-0.3Fe-0.1P. Chemical Composition, wt (Nominal) Iron 0.3 Phosphorus 0.01 Copper bal Physical...