Alloy Digest (2017) 66 (1): Cu-856.
Published: 01 January 2017
... Alloy KHP 102 (UNS C19010) is a high performance copper alloy with additions for strength while maintaining high conductivity. KHP 102 belongs to the group of CuNiSi alloys and is particularly suitable for use in electrical and electronic products. This datasheet provides information...
Journal Articles
Alloy Digest (2019) 68 (3): cu-885.
Published: 01 March 2019
...: Olin Brass Copyright ┬ę ASM International┬« 2019 2019 ASM International chemical composition electrical conductivity OLIN BRASS ALLOY C19010 physical properties tensile properties thermal properties UNS C19010 Olin Brass Alloy C19010 is a silicon bronze precipitation hardened alloy...
Journal Articles
Alloy Digest (2015) 64 (7): Cu-839.
Published: 01 July 2015
... elasticity electrical applications fabricability fatigue properties hardness heat treatability joinability physical properties tensile properties Wieland-K76 workability thermal properties UNS C19010 Wieland-K76 is copper alloyed with low nickel for good fabricability for parts...