Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (9): Cu-812.
Published: 01 September 2012
... electronic applications joinability machinability physical properties tensile properties Wieland-K62 workability UNS C18090 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2012, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final design...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (3): Cu-558.
Published: 01 March 1991
... International chemical composition Copper alloy no. C18090 elasticity electrical conductivity heat treatability joinability machinability physical properties workability UNS C18090 - DIGEST- COPPER ALLOY Cl8090 t?& cu-558 I I DATA ON WORLD WIDE METALS AND ALLOYS MARCH 1991 cc4q7@M1991...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (2): Cu-569.
Published: 01 February 1992
... alloy no. C18090 elasticity fatigue properties heat treatability joinability machinability physical properties tensile properties workability UNS C18090 COPPER ALLOY NO. C18()9() y cu-56g - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS FEBRUARY 1992 @C@yn@l1992, Al&y LJ@esf. Inc. All r@hfs I...