Alloy Digest (1999) 48 (10): Cu-641.
Published: 01 October 1999
... resistance thermal properties UNS C17530 BERYLCO® 7 (Beryllium Copper Precipitation-Hardening Alloy) Berylco 7 is beryllium copper alloy with 0.3 % beryllium. The alloy has high conductivity, fatigue strength, and wear resistance and is nonmag- netic. Berylco is a registered trademark of NGK Metals Corp...
Journal Articles
Alloy Digest (1999) 48 (11): Cu-642.
Published: 01 November 1999
... the same level of reliability. The electrical conductivity of C17530 is 38% mini- mum of IACS. Beryllium copper alloys are good choices for high current density springs requiring low heat generation. Be- ryllium copper has good corrosion resistance, nearly equal to that of nickel silver. Spring Properties...