Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
... workability thermal properties UNS C17500-C17510 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2010, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151...
Journal Articles
Alloy Digest (2000) 49 (10): Cu-29.
Published: 01 October 2000
... joinability machinability physical properties tensile strength thermal conductivity workability UNS C17500 C17510 CMW 100 is a copper alloy that combines high tensile strength with high electrical and thermal conductivity. It responds to age-hardening heat treatment. It is used for flash welding dies...