Alloy Digest (2010) 59 (12): Cu-792.
Published: 01 December 2010
...-792. Producer or source: PMX Industries Inc. Producer or Source: PMX Industries Inc. Copyright © ASM International® 2010 2010 ASM International bend strength chemical composition PMX ALLOY C14530 tensile properties workability UNS C14530 DATA ON WORLDWIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (2003) 52 (5): Cu-702.
Published: 01 May 2003
... UNS C14530 Chemical Composition, wt Copper, including silver, tin, tellurium, 99.90 and/or selenium Tin 0.003 0.023 Tellurium or selenium 0.003 0.023 Phosphorus 0.001 0.01 Physical Properties: Density, kg/m3 (lb/in.3 ) 8900 (0.323) Coefficient of linear thermal 17.7 (9.8) expansion, 10 6/K (10 6/°F...
Journal Articles
Alloy Digest (2008) 57 (6): Cu-755.
Published: 01 June 2008
... heat-transfer applications joinability LUVATA C1453 machinability physical properties tensile properties workability thermal properties UNS C14530 LUVATA C1453 (Copper Tellurium Alloy) Luvata C1453 (CuTe0.02Sn0.02) is a patented copper tellurium alloy for electrical and heat-transfer...
Journal Articles
Alloy Digest (1999) 48 (4): Cu-632.
Published: 01 April 1999
...-632B 2.5 2 1.5 1 0.5 0 Ba d wa y be nd fo rm a bi lity (M BR /t) 30 35 40 45 50 55 60 65 70 0.2% offset yield strength (ksi) C110 C151 Fig. 1 Formability and strength of C110 and C151 Fig. 2 Stress relaxation resistance of C151 C110 Hd C260 Hd C14530 Spr C194 Hd C151 Hd 100 90 80 70 60 50 40 30 20 10 0...