Alloy Digest (1986) 35 (1): Al-264.
Published: 01 January 1986
.... Specification Equivalents: UNS No. A96010. General Characteristics: ALCOA 6010 ALLOY sheet can be formed on thesameprssesand at similar line speeds as steel and on-line repairs can also be handled with the same speed and similar procedures as for steel. The yield strength of alloy 6010 increases to 45000 psi...