Alloy Digest (2022) 71 (2): Al-485.
Published: 01 February 2022
... Austral Wright 3003 (UNS A93003) is a wrought, non-heat-treatable, aluminum-manganese-copper alloy (3xxx series). It is used in a wide variety of applications where moderate strength, good formability, and good resistance to corrosion are important. This datasheet provides information...
Journal Articles
Alloy Digest (2021) 70 (6): Al-477.
Published: 01 June 2021
... Steels. Producer or Source: Atlas Steels Copyright ┬ę ASM International┬« 2021 2021 ASM International Atlas Steels 3003 chemical composition corrosion resistance forming heat treating joining machining physical properties tensile properties thermal properties UNS A93003 ATLAS...
Journal Articles
Alloy Digest (1987) 36 (11): Al-284.
Published: 01 November 1987
.... Federal: QQ-A-200, QQ-A-225; QQ-A-250; QQ-A4N and WWT-700. Military: MIL-S-12875; MIL-E-15597; MIL-P-25995; MIL-A52174; MIL-A-81596. SAE: J454. UNS No. A93003. General Characteristics: AA 3003is an general purpose alloy, slightlystrongerthan AA I 100 and it hasvery good drawin& forming and welding...