Skip Nav Destination
Close Modal
Search Results for
UNS A91350
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
UNS A91350
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (3): Al-302.
Published: 01 March 1990
... joinability machinability physical properties shear strength tensile properties workability UNS A91350 AA 1350 Filing Code: AI-302 Aluminum Alloy - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS MARCH 1990 -by: AloyUigost, lnc1ZOl-6%6161 27CMI6OldStrrl~N.J.070601U.SA AA 1350 (GonduetorGradeAluminum) AA...
Abstract
View article
PDF
AA 1350, formerly designated EC, is an electrical conductor grade aluminum. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Al-302. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (7): Al-395.
Published: 01 July 2005
... chemical composition corrosion-resistant alloys joinability machinability physical properties shear strength tensile properties workability thermal properties UNS A91060, A91100, A91350 Chemical Composition, wt (Typical) Alloy 1060 Alloy 1100 Alloy 1350 Silicon 0.25 max 0.95 min (Si + Fe) 0.10...
Abstract
View article
PDF
Aluminum 1xxx series alloys are nonhardenable by heat treatment. They have high purity, high conductivity, and good corrosion resistance and are easily formed. This datasheet provides information on composition, physical properties, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: AL-395. Producer or source: Alcoa Engineered Products.