Publisher: Journals Gateway
Alloy Digest (2004) 53 (6): Al-389.
Published: 01 June 2004
... physical properties UNS A25240 Chemical Composition, wt Chromium 0.05 max Copper 4 4.5 Iron 0.12 max Silicon 0.06 max Titanium 0.1 max Zirconium 0.15 max Magnesium 1.2 1.6 Manganese 0.45 0.7 Other, each 0.05 max Other, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3 ) 2780 (0.1...