Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... properties tensile properties valves UNS A07070 APEX TERNALLOY 7 Filing Code: Al-279 Aluminum Alloy APRIL 1987 - DATA ON WORLD WIDE METALS AND ALLOYS Published by Alloy Digest. Inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 APEX TERNALLOY 7 (Aluminum Foundry Alloy) APEX TERNALLOY 7 is...
Journal Articles
Alloy Digest (1985) 34 (9): Al-260.
Published: 01 September 1985
... corrosion-resistant alloys elasticity hardness heat treatability joinability machinability manifolds physical properties pipe fittings tensile properties valves UNS A07070 ALUMINUM 707.0 Filing Code: AI-260 Aluminum Alloy SEPTEMBER 1966 - DATA ON WORLD WIDE METALS AND ALLOYS a Copyrtgh! 1985...