Alloy Digest (1983) 32 (1): Al-242.
Published: 01 January 1983
... be treated by one of a number of specialized surface treatments for aluminum alloys; however, it is difficult to attain a uniform appearance after anodizing. Consult manufacturers for more details on surface treatments. Specification Equivalents: ASTM B 85. UNS No. A05180. Federal: QQ-A-59 I. Former...