1-20 of 2182 Search Results for

UNS -

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (4): CS-104.
Published: 01 April 1985
... UNS No. G10460 is a general-purpose construction and machinery steel. It can be used in a variety of conditions: hot rolled, annealed, normalized, oil quenched and tempered, water quenched and tempered or austempered. It furnishes medium strength and toughness at a low cost. It is frequently used...
Journal Articles
Alloy Digest (1985) 34 (6): TS-443.
Published: 01 June 1985
... UNS No. T11304 was developed to provide the excellent abrasion resistance that results from higher-than-normal carbon and vanadium in the molybdenum-tungsten high-speed steels. It is a high-hardenability steel and is recommended where sharp edges are needed for fine cuts. It is an excellent choice...
Journal Articles
Alloy Digest (1985) 34 (5): CS-105.
Published: 01 May 1985
... UNS No. G10780 is a plain carbon steel; it has low hardenability and a high carbon content (nominally 0.78%). It can be hardened by quenching into oil or water from the austenitizing temperature; care must be exercised to prevent cracking when quenching into water. This steel develops high surface...
Journal Articles
Alloy Digest (1985) 34 (8): CS-108.
Published: 01 August 1985
... UNS No. G10160 is a carburizing and general-purpose steel. It is a low-carbon steel that combines good machinability, good workability and good weldability. It is used for components case-hardened by carburizing. It is used in the hot-rolled, annealed, normalized or cold-worked condition...
Journal Articles
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... UNS No. T20812 is a low-carbon chromium-molybdenum-tungsten hot-work steel for general purposers. It is used for dies and tools that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat...
Journal Articles
Alloy Digest (1986) 35 (3): SA-416.
Published: 01 March 1986
... UNS No. H51321 is a medium-hardenability, through-hardening steel of low (0.75-1.00%) chromium content. It is recommended for uses where moderate strength and toughness are satisfactory. It may be used in the unhardened condition or after quenching in water or oil followed by tempering...
Journal Articles
Alloy Digest (1986) 35 (7): Al-269.
Published: 01 July 1986
... UNS No. A97075 is a wrought precipitation-hardenable aluminum alloy. It has excellent mechanical properties, workability and response to heat treatment and refrigeration. Its typical uses comprise aircraft structural parts and other highly stressed structural applications where very high strength...
Journal Articles
Alloy Digest (1986) 35 (8): CS-112.
Published: 01 August 1986
... UNS No. G10860 is a high-carbon oil or water-hardening steel of low hardenability. It develops high surface hardness on quenching rapidly and tempering lightly and it has good resistance to wear. It is used for tools, springs, music wire, machinery parts and many other applications. This datasheet...
Journal Articles
Alloy Digest (1986) 35 (10): Cu-516.
Published: 01 October 1986
... International® 1996 1996 ASM International BRUSH PHOSPHOR BRONZE chemical composition corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability physical properties tensile properties workability UNS C51000 1 BRUSH PHOSPHOR BRONZE 1 Fi ing Ode: c -516...
Journal Articles
Alloy Digest (1986) 35 (10): Al-272.
Published: 01 October 1986
... UNS No. A02220 is an age-hardenable aluminum casting alloy. It is hard and wear resistant and has good strength at elevated temperatures. It has good foundry characteristics in many respects and is produced as sand and permanent-mold castings. Among its applications are bushings, automotive...
Journal Articles
Alloy Digest (1986) 35 (12): Al-274.
Published: 01 December 1986
... UNS No. A03560 is a heat-treatable aluminum casting alloy. Normally it is used only when heat-treated (aged) strengths are required. It is recommended for high-strength, pressure-tight castings, intricate shapes and where good resistance to corrosion is needed. Its many applications include crank...
Journal Articles
Alloy Digest (1988) 37 (1): Al-286.
Published: 01 January 1988
... UNS No. A02080 is a heat-treatable casting alloy characterized by good castability, machinability and resistance to corrosion. It is produced by sand casting and is a general-purpose alloy recommended in both the as-cast and heat-treated conditions. This datasheet provides information...
Journal Articles
Alloy Digest (1988) 37 (2): SA-427.
Published: 01 February 1988
... UNS H41370 is a low-alloy steel containing nominally 0.95% Cr and 0.20% Mo. It has good resistance to abrasion, fatigue, and impact. It can be nitrided successfully for maximum resistance to abrasion and wear. It is suitable for severe service characterized by high stresses and impact loading...
Journal Articles
Alloy Digest (1988) 37 (2): Cu-535.
Published: 01 February 1988
... UNS No. C16200 is a copper-cadmium alloy with high electrical and thermal conductivities combined with high strength and toughness. It is recommended for resistance-welding electrodes, back-up bars and current carrying rings. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1988) 37 (3): SA-428.
Published: 01 March 1988
... UNS NO. H40470 is a molybdenum (0.20-0.30%) alloy steel of moderate hardness and strength. It has good toughness in the quenched-and tempered condition because it is relatively free from temper embrittlement when tempered in the susceptible range of approximately 850-1100 F. The automotive...
Journal Articles
Alloy Digest (1988) 37 (3): Cu-536.
Published: 01 March 1988
... UNS NO. C36000 is a leaded brass suitable for high-speed screw-machine work. It has many uses such as hardware, gears and pinions. Its trade names include free-turning brass, free-cutting yellow brass and high-leaded brass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1988) 37 (3): Al-287.
Published: 01 March 1988
... UNS NO. A96101 in the heat treated condition is used primarily for enclosed bus conductor where both high strength and high electrical conductivity are desirable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1988) 37 (3): Zn-42.
Published: 01 March 1988
... UNS No. Z35635 is a zinc-aluminum-copper-magnesium foundry alloy recommended for castings of moderate strength and low cost. It was designed for use in nonferrous permanent-mold foundries to compete with cast-iron, aluminum and bronze castings. The alloy can be sand cast and die cast. Its many...
Journal Articles
Alloy Digest (1988) 37 (4): TS-489.
Published: 01 April 1988
... UNS No. T30106 is an air-hardening high-carbon tool steel designed for a combination of high strength, good wear resistance, and good toughness. It is easy to heat treat with a minimum of distortion and is used extensively for plastic molds. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1988) 37 (5): Cu-538.
Published: 01 May 1988
... UNS No. C10100 is a wrought oxygen-free, high-conductivity copper for electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information...