Alloy Digest (1960) 9 (7): SS-105.
Published: 01 July 1960
... UNITEMP 212 is a precipitation hardening steel that will maintain high strength and corrosion resistance up to 1400 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also...
Journal Articles
Alloy Digest (1987) 36 (2): Ni-344.
Published: 01 February 1987
... UNITEMP 625 is a nickel-base, austenitic, solution-strengthened high-performance alloy that provides excellent resistance to both high-temperature gaseous corrosion and aqueous corrosion coupled with good strength and stress-rupture properties to 1800 F. The alloy has good resistance to stress...
Journal Articles
Alloy Digest (1959) 8 (2): Co-15.
Published: 01 February 1959
... UNITEMP L-605 is a cobalt-base alloy having the highest strength at high temperatures above about 1600 deg F. It is used only where high stresses exist at the upper end of the temperature range of 1700 deg F to 2000 deg F. See the updated version, Alloy Digest Co-69, revised July 1990. This...
Journal Articles
Alloy Digest (1974) 23 (3): Ni-46.
Published: 01 March 1974
... UNITEMP WASPALOY is a nickel-base, austenitic precipitation-hardenable alloy. It has excellent strength and good resistance to corrosion and oxidation at temperatures at least to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...