Alloy Digest (1974) 23 (5): SA-304.
Published: 01 May 1974
... UNIMAR 250 is a maraging alloy steel having high strength, good notch toughness, excellent cryogenic properties and deep hardenability. It is recommended for pressure vessels, solid-fuel rocket cases and pressure bottles, landing-gear components, processing equipment operating in the temperature...