1-1 of 1 Search Results for

UNILOY EB 26-1

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1971) 20 (9): SS-260.
Published: 01 September 1971
... UNILOY EB 26-1 is a stainless steel alloy produced by the electron-beam refining (EBR) process. It is an extremely high-purity ferritic stainless steel, having an attractive combination of strength, ductility, fabricability, and corrosion resistance. This datasheet provides information...