1-1 of 1 Search Results for

UNIFLUX VCM 225

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1978) 27 (3): SA-344.
Published: 01 March 1978
... UNIFLUX VCM 225 is a continuous flux-cored welding electrode (wire) that is used to deposit 2-1/4% chromium-1% molybdenum steel weld when used to weld 2-1/4% chromium-1% molybdenum steel for which it was developed. Welding is protected by a shielding atmosphere of 100% carbon dioxide...