1-1 of 1 Search Results for

UMCo-51

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1967) 16 (3): Co-51.
Published: 01 March 1967
... UMCo-51 is a cobalt-base alloy having high stress-rupture strength. It is recommended for high temperature applications where the mechanical stresses are high, and where resistance to abrasion, thermal shock and oxidation are required. This datasheet provides information on composition, physical...