Skip Nav Destination
Close Modal
Search Results for
ULTRONZE
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
ULTRONZE
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
... ULTRONZE is a copper alloy also known as Olin Alloy 654. It bridges the gap between standard high-performance copper alloys and beryllium-copper alloys, thus enabling the design of parts with properties previously only attainable with more expensive materials. The alloy has superior stress...
Abstract
View article
PDF
ULTRONZE is a copper alloy also known as Olin Alloy 654. It bridges the gap between standard high-performance copper alloys and beryllium-copper alloys, thus enabling the design of parts with properties previously only attainable with more expensive materials. The alloy has superior stress-relaxation characteristics, good bend performance and excellent corrosion resistance. Among its typical uses are electrical connectors, fuse clips and relay springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Cu-417. Producer or source: Olin Brass.