Alloy Digest (1990) 39 (7): Cp-16.
Published: 01 July 1990
... ULTEM 6100 and 6200 are glass reinforced and ULTEM 6202 is a mineral filled copolymer resin. For properties of the unreinforced resin, ULTEM 6000, see Alloy Digest P-27, June 1991. These are high temperature materials that are particularly suitable for military electrical components which must...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (2): Cp-5.
Published: 01 February 1990
... ULTEM 2100, 2200, 2300 and 2400 resins have high heat resistance, inherent flame resistance with low smoke evolution, broad chemical resistance and outstanding processability. Glass reinforcment provides increased rigidity and dimensional stability while maintaining good processing features...