Alloy Digest (1990) 39 (7): Cp-16.
Published: 01 July 1990
... ULTEM 6100 and 6200 are glass reinforced and ULTEM 6202 is a mineral filled copolymer resin. For properties of the unreinforced resin, ULTEM 6000, see Alloy Digest P-27, June 1991. These are high temperature materials that are particularly suitable for military electrical components which must...