Alloy Digest (1990) 39 (2): Cp-5.
Published: 01 February 1990
... ULTEM 2100, 2200, 2300 and 2400 resins have high heat resistance, inherent flame resistance with low smoke evolution, broad chemical resistance and outstanding processability. Glass reinforcment provides increased rigidity and dimensional stability while maintaining good processing features...