Alloy Digest (1977) 26 (1): SS-336.
Published: 01 January 1977
... UHB Stainless 34L is noted for its extra-low carbon content (0.03% max) and high molybdenum content (4.3%). It has excellent resistance to uniform corrosion and to pitting corrosion. Its tensile strength is approximately the same as that of other austenitic stainless steels. This steel...