1-1 of 1

Search Results for UHB RIGOR A2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (3): TS-315.
Published: 01 March 1977
... UHB RIGOR A2 wear resistance workability UHB RIGOR A2 Filing Code: TS-315 Tool Steel MARCH 1977 - DATA ON WORLD WIDE METALS AND ALLOYS UHB RIGOR+ A2 Psbiirbd by Eogineering AIIOYS Digest Inc. (Air-Hardening Cold Work Steel; AISI Type A21 Upper MontcZr, New Jw UHB RIGOR AR is a chromium-molybdenum...