Journal Articles
Alloy Digest (1975) 24 (10): TS-291.
Published: 01 October 1975
... UHB Regin 3 is a chromium-tungsten-vanadium tool steel characterized by good toughness (especially when exposed to impact stresses), high red hardness, good wear resistance and good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity...