Publisher: Journals Gateway
Alloy Digest (1999) 48 (8): SS-754.
Published: 01 August 1999
... UGINA 4567 and 304Cu are the same grades designated differently for the European and North American markets, respectively. Controlled steelmaking results in machining gains, particularly in deep drilling, over UGIMA 4307 (see Alloy Digest SS-722, November 1998). This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (8): SS-1350.
Published: 01 August 2022
... is produced that offers good machinability. This improved machinability grade (referred to as Ugima 4567) is available only by special order, but it should be considered as an option where an 18/8 austenitic stainless steel is specified that needs to be both heavily cold formed and extensively machined...