1-4 of 4 Search Results for

UGIMA 4404

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (12): SS-735.
Published: 01 December 1998
... UGIMA 4404 (UGIMA 316L) is identical to UGINE 4404 (AISI 316L) in analysis, corrosion resistance, mechanical properties, and forging and welding ability, but not with respect to machinability. A specific melting process creates inclusions of malleable oxides with a low melting point. The...
Journal Articles
Alloy Digest (2013) 62 (9): SS-1156.
Published: 01 September 2013
... Ugima 440 HM is a general-purpose, corrosion resistant austenitic stainless steel with added molybdenum (300 series with 2–2.5% Mo). It features improved machinability compared with 4404 or 316L. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (2014) 63 (4): SS-1170.
Published: 01 April 2014
... sulfur percentage of approximately 0.015% and controlled sulfide inclusion populations, this alloy offers good machining performance, but without achieving the exceptional machinability levels of UGIMA 4404HM. Corrosion Resistance: UGI 4404 FGX3 has very good corrosion resistance. As is the case with the...
Journal Articles
Alloy Digest (2018) 67 (6): SS-1289.
Published: 01 June 2018
... than EN 4462 and equivalent to UGIMA 4404. Drilling. Ø4 mm (0.16 in.) high-speed steel drill) for Ø4 mm (0.16 in.) drilling, chip containment creates the same problem with respect to chip removal as that observed with Duplex 4462, due to poor chip breakability. Max chip flow for 1140 holes 16 mm (0.63...