Alloy Digest (1998) 47 (11): SS-734.
Published: 01 November 1998
... UGIMA 4401 (UGIMA 316) is identical to UGINE 4401 (AISI 316) in analysis, corrosion resistance, mechanical properties, and forging and welding abilities but dissimilar in machinability. A specific melting process creates inclusions (malleable oxides with a low melting point), which improve...