Alloy Digest (2013) 62 (12): SS-1163.
Published: 01 December 2013
... Ugima 4307 HM is a general-purpose, corrosion resistant austenitic stainless steel with improved machinability. Its corrosion resistance is typical of an austenitic steel and is similar to that of 4307 or 304L. This datasheet provides information on composition, physical properties, elasticity...