Alloy Digest (2018) 67 (10): SS-1296.
Published: 01 October 2018
... UGI 4418 AIR is a martensitic stainless steel with strong corrosion resistance and mechanical performance. It is used for parts requiring a combination of high strength and high toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2018) 67 (8): SS-1292.
Published: 01 August 2018
...). Quenching. Oil quenching (or air quenching depending on the cross-sections) from 950 °C to 1050 °C (1742 1922 °F). Copyright © 2018, ASM International®. All rights reserved. UGI 4418 (Martensitic Stainless Steel) Filing Code: SS-1292 Stainless Steel :: August 2018 Materials Park, Ohio 44073-0002...