Alloy Digest (1972) 21 (4): Ni-171.
Published: 01 April 1972
... UDIMET 75 is a nickel-base high-temperature alloy developed for good resistance to oxidation and scaling to 2000 F. It can be fabricated and welded readily. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (2004) 53 (12): Co-109.
Published: 01 December 2004
... Udimet L-605 is a high-temperature aerospace alloy with excellent strength and oxidation resistance. It is used in applications such as gas turbine blades and combustion area parts. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It...
Journal Articles
Alloy Digest (2005) 54 (1): Co-110.
Published: 01 January 2005
... Udimet 188 is a high-temperature aerospace alloy with excellent strength and oxidation resistance. It is used in applications such as gas turbine blades and combustion area parts. The alloy has a tenacious oxide film. This datasheet provides information on composition, physical properties, and...
Journal Articles
Alloy Digest (1987) 36 (1): Ni-51.
Published: 01 January 1987
... UDIMET 700 is a wrought nickel-base alloy produced by vacuum-induction melting and further refined by vacuum-arc remelting. It has excellent mechanical properties at high temperatures. Among its applications are blades for aircraft, marine and land-based gas turbines and rotor discs. This...
Journal Articles
Alloy Digest (1963) 12 (1): SA-139.
Published: 01 January 1963
... Udimet A is a vacuum induction melted high strength steel designed to achieve yield strengths in excess of 250,000 psi with conventional thermal treatment while maintaining excellent ductility. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (2020) 69 (5): Co-131.
Published: 01 May 2020
...) 12.3 (6.8) (a) Thermal conductivity W/(m K) (Btu/(h·ft·°F)) 9.4 (5.4) Specific heat capacity J/(kg K) (cal/(g °C)) 21 °C (70 °F) 385 (0.092) Electrical resistivity m circular-mil/ft) 24 °C (75 °F) 0.886 (533.2) Magnetic permeability(b) 1.002 Typical values. RT = room temperature. (a) Source: ATI...