Skip Nav Destination
Close Modal
Search Results for
U.S.S. COR-TEN
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
U.S.S. COR-TEN
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (11): SA-283.
Published: 01 November 1972
... USS COR-TEN A, the original COR-TEN Steel composition (see U.S.S. COR-TEN, Alloy Digest SA-17, April 1954), has 5 to 8 times the atmospheric corrosion resistance of structural carbon steel and a minimum yield point of 50,000 psi in sections through 1/2-inch thick. This datasheet provides...
Abstract
View article
PDF
USS COR-TEN A, the original COR-TEN Steel composition (see U.S.S. COR-TEN, Alloy Digest SA-17, April 1954), has 5 to 8 times the atmospheric corrosion resistance of structural carbon steel and a minimum yield point of 50,000 psi in sections through 1/2-inch thick. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-283. Producer or source: United States Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (4): SA-17.
Published: 01 April 1954
... U.S.S. COR-TEN is a corrosion resistant high-strength steel of low alloy content, intended primarily for weight reduction, or longer life, by means of greater strength and enhanced atmospheric corrosion resistance in applications involving fabrication by forming and welding. This datasheet...
Abstract
View article
PDF
U.S.S. COR-TEN is a corrosion resistant high-strength steel of low alloy content, intended primarily for weight reduction, or longer life, by means of greater strength and enhanced atmospheric corrosion resistance in applications involving fabrication by forming and welding. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-17. Producer or source: United States Steel Corporation.