Alloy Digest (1961) 10 (11): Cu-110.
Published: 01 November 1961
... Tuf-Stuf 224E-30 is a general purpose alloy for use where high strength and corrosion resistance are necessary, but where high hardness is not a factor. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1962) 11 (11): Cu-122.
Published: 01 November 1962
... 4630 MIL-B-15939, Comp. 1 Fed. QQ-A-630 Comp. 1 ASTM B124, Alloy lla; B150, Alloy 1 SAE 701B General Characteri sties: TUF-STUF 224E-75 is a general purpose aluminum bronze possessing high tensile strength and good corrosion resistance. It has higher hardness than TUF-STUF 224E-30, and offers strength...