Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... with wear resistance in these severe loading conditions. ToughMet 2CX in the cast and spinodally hardened (CX) condition exhibits tensile strength in excess of 724 MPa (105 ksi) and hardness exceeding HRC 27 with excellent machinability. This datasheet provides information on composition, physical...