Alloy Digest (2013) 62 (5): Cu-724.
Published: 01 May 2013
... ToughMet 2 is a high performance, wrought, heat treatable, lead-free strip Cu-Ni alloy that imparts superior mechanical performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. ToughMet alloys...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... ToughMet 2 CX is a Cu-9Ni-6Sn alloy that combines low coefficient of friction with wear resistance. ToughMet alloys are a line of spinodal hardened Cu-Ni antigalling alloys for bearings capable of performing with a variety of shafting materials and lubricants. The alloys combine a high lubricity...
Journal Articles
Alloy Digest (2001) 50 (7): Cu-670.
Published: 01 July 2001
... 1100 (65 160) Elongation, % 2 45 Young s modulus, GPa (106 psi) 117 128 (17 18.5) Hardness, HRC 20 36 Impact toughness, Charpy V-notch, J (ft · lbf) 8 271 (8 271) Fatigue strength, 108 cycles, R = 1, MPa (ksi) 172 415 (25 60) The ToughMet alloy system property ranges are shown above, and mini- mum...