Skip Nav Destination
Close Modal
Search Results for
Titanium-Aluminum-Vanadium-Chromium-Molybdenum-Zirconium
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-14 of 14
Search Results for Titanium-Aluminum-Vanadium-Chromium-Molybdenum-Zirconium
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2002) 51 (9): Ti-130.
Published: 01 September 2002
... properties heat treatability high-temperature alloys joinability machinability physical properties shear strength tensile properties Titanium-Aluminum-Vanadium-Chromium-Molybdenum-Zirconium workability thermal properties Chemical Composition, wt (Typical analysis, AMS 4957 rev. B and AMS 4958...
Abstract
View articletitled, Ti 3Al-8V-6Cr-4Mo-4Zr: Age-Hardenable <span class="search-highlight">Titanium</span> Alloy
View
PDF
for article titled, Ti 3Al-8V-6Cr-4Mo-4Zr: Age-Hardenable <span class="search-highlight">Titanium</span> Alloy
Carpenter titanium alloy Ti 3Al-8V-6Cr-4Mo-4Zr, or Ti-3-8-6-4-4, is a beta alloy that contains large amounts of beta stabilizers (molybdenum and vanadium) and can be heat treated. The alloy is commonly known as Beta C. A specialized application for this alloy is aircraft springs. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-130. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2005) 54 (6): Ti-94.
Published: 01 June 2005
...-Molybdenum weldability workability thermal properties UNS R58640 Composition, wt Carbon 0.05 max Nitrogen 0.03 max Oxygen 0.14 ma Iron 0.03 max Aluminum 3.0 4.0 Vanadium 7.5 8.5 Chromium 5.5 6.5 Zirconium 3.5 4.5 Molybdenum 3.5 4.5 Titanium bal Physical Properties: Density, kg/m3 (lb/in.3 ) 4816...
Abstract
View articletitled, Ti-3Al-8V-6Cr-4Zr-4Mo: Heat Treatable Beta <span class="search-highlight">Titanium</span> Alloy
View
PDF
for article titled, Ti-3Al-8V-6Cr-4Zr-4Mo: Heat Treatable Beta <span class="search-highlight">Titanium</span> Alloy
Ti-3Al-8V-6Cr-4Zr-4Mo alloy is a heat treatable beta grade titanium alloy. It is a high-strength alloy with fair weldability and is easier to melt than 13-11-3. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-94. Producer or source: Titanium alloys mills. Originally published as Ti-3Al-8V-6Cr-4Zr-4Mo BETA ALLOY, January 1990, revised June 2005.
Journal Articles
Alloy Digest (1994) 43 (8): Ni-461.
Published: 01 August 1994
... Silicon Nickel Cobalt Manganese Phosphorus SUlhU Vanadium Nickel & Molybdenum Aluminum Columbium (Nb) Copper Tantalum Titanium Tungsten Zirconium 1.0-3.0 1.0-3.0 27.0-32.0 0.01 max. 0.10 max. 65.0 min. 3.0 max. 3.0 max. 0.030 max. 0.010 max. 0.20 max. 94.0-98.0 0.50 max. 0.20 max. 0.20 max. 0.20 max. 0.20...
Abstract
View articletitled, HASTELLOY B-3 ALLOY: Corrosion Resistant Nickel-Base Alloy
View
PDF
for article titled, HASTELLOY B-3 ALLOY: Corrosion Resistant Nickel-Base Alloy
HASTELLOY B-3 ALLOY is a nickel-molybdenum alloy with thermal stability to reduce the deleterious intermetallic precipitates which cause loss of ductility and corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-461. Producer or source: Haynes International Inc.
Journal Articles
Alloy Digest (1987) 36 (8): Ti-87.
Published: 01 August 1987
..., rivets and downhole oil-production equipment. *RMl is a registered trademark of the RMI Company. Common: Aluminum Vanadium Chromium Molybdenum Zirconium lr0fi Nitrogen Carbon Oxygen Hydrogen Others. total each i itantum 3.0-4.0 7.5-8.5 5.5-6.5 3.5-4.5 3.5-4.5 0.30 max. 0.03 max. 0.05 max. 0.12 max. 0.020...
Abstract
View articletitled, RMI BETA-C: Corrosion Resistant Alloy
View
PDF
for article titled, RMI BETA-C: Corrosion Resistant Alloy
RMI Beta C is a heat-treatable titanium-base alloy that develops a tensile strength of over 200,000 psi in the solution-treated-and-aged condition. It has good ductility and toughness, good fabricability and a low elastic modulus. It has good resistance to general corrosion and it resists hot, aggressive environments containing ferric chloride, sodium chloride, carbon dioxide and hydrogen sulfide. Its applications include coil springs, fasteners, rivets and downhole oil-production equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-87. Producer or source: RMI Company.
Journal Articles
Alloy Digest (1994) 43 (3): Hf-1.
Published: 01 March 1994
... Magnesium Manganese Nickel Nimogen Oxygen Silicon Titanium Uranium Zirconium Copper Molybdenum Tungsten Columbium Hydrogen Tantalum Vanadium Sponge crystal Rod & Sheet, Plate Bar Wire & strip - - 200 70 100 100 100 30 150 150 200 100 20 100 100 750 250 250 250 600 50 50 50 50 50 50 10 100 100 1500 100 400...
Abstract
View articletitled, HAFNIUM: Element No. 72
View
PDF
for article titled, HAFNIUM: Element No. 72
HAFNIUM is a commercially available refractory metal which has outstanding corrosion resistance, good mechanical properties, and is readily amenable to standard fabrication techniques. These characteristics, coupled with its high thermal-neutron cross section, high-temperature allotropic transformation, and excellent electrical properties, have made it of increasing interest to design engineers in a variety of fields. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information on corrosion resistance as well as machining and joining. Filing Code: HF-1. Producer or source: Teledyne Wah Chang Albany.
Journal Articles
Alloy Digest (2001) 50 (12): Ti-124.
Published: 01 December 2001
... Vanadium 7.5 8.5 Chromium 5.5 6.5 Zirconium 3.5 4.5 Molybdenum 3.5 4.5 Iron 0.3 max Carbon 0.05 max Oxygen 0.12 max Palladium 0.04 0.08 Nitrogen 0.03 max Hydrogen 0.02 max Titanium bal Physical Properties: Density, kg/m3 (lb/in.3 ) 4820 (0.174) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 0...
Abstract
View articletitled, RMI Ti BETA-C/Pd: Corrosion-Resistant Alloy
View
PDF
for article titled, RMI Ti BETA-C/Pd: Corrosion-Resistant Alloy
RMI Ti Beta-C/Pd alloy is a Ti-3Al-8V-6Cr-4Zr-4Mo-0.05Pd alloy also referred to as Grade 20. It is a palladium-containing version of RMI Beta-C alloy possessing equivalent physical and mechanical properties, but with enhanced corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fracture toughness and creep. It also includes information on high temperature performance. Filing Code: TI-124. Producer or source: RMI Company.
Journal Articles
Alloy Digest (2004) 53 (7): Ti-134.
Published: 01 July 2004
... ductility elasticity hardness heat treatability joinability machinability physical properties tensile properties workability thermal properties UNS R58640 Chemical Composition, wt Aluminum 3.0 4.0 Vanadium 7.5 8.5 Chromium 5.5 6.5 Molybdenum 3.5 4.5 Zirconium 3.5 4.5 Iron 0.35 max Oxygen 0.12...
Abstract
View articletitled, ALLVAC 38-644: Beta <span class="search-highlight">Titanium</span> Alloy
View
PDF
for article titled, ALLVAC 38-644: Beta <span class="search-highlight">Titanium</span> Alloy
Allvac 38-644 is a metastable beta titanium alloy known for its ductility in the solution treated condition and its high strength and ductility in the solution treated and aged condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TI-134. Producer or source: Allvac Metals Company.
Journal Articles
Alloy Digest (2011) 60 (2): SA-620.
Published: 01 February 2011
... 0.01 Silicon 0.05 0.50 Nickel 0.75 Chromium 0.25 Molybdenum 0.08 Copper 0.35 Titanium 0.007 0.02 Columbium 0.03 Nitrogen(c, d) 0.12 Aluminum (acid sol) 0.015 0.055 Aluminum (total) 0.02 0.06 Boron(c) 0.001 (a) Values are maximums unless a range is shown. (b) Mn up to 1.65% (heat analysis) is permitted...
Abstract
View articletitled, DOGAL API 2W GRADE 50: Thermomechanical Control Processed Plate
View
PDF
for article titled, DOGAL API 2W GRADE 50: Thermomechanical Control Processed Plate
DOGAL API 2W GRADE 50 is thermomechanical control processed plate produced to meet specifications for API 2W Grade 50 Steel. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-620. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
Alloy Digest (2019) 68 (12): SA-857.
Published: 01 December 2019
... temperatures. Aldur® is a trademark of Voestalpine Grobblech GmbH Chemical Composition, wt.% (Typical, maximum) Carbon 0.20 Silicon 0.80 Manganese 1.70 Phosphorus 0.020 Sulfur 0.010 Aluminum, total 0.018 min Nitrogen 0.015 Vanadium 0.12 Niobium 0.06 Titanium 0.05 Zirconium 0.15 Chromium 1.50 Copper 0.50 Nickel...
Abstract
View articletitled, ALDUR 900Q, QL: Structural Steel
View
PDF
for article titled, ALDUR 900Q, QL: Structural Steel
Aldur 900 steels (minimum yield strength of 900 MPa, or 131 ksi, for thicknesses up to 50 mm, or 2 in.) are a part of a family of waterquenched, high-strength, fine-grained steels that have excellent toughness at low temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low temperature performance. Filing Code: SA-857. Producer or source: Voestalpine Grobblech GmbH.
Journal Articles
Alloy Digest (1966) 15 (10): Ni-118.
Published: 01 October 1966
... Zirconium 0.05-O. 15 Chromium 11.0-13.0 Molybdenum 3.8-5.2 Titanium 0.4-1.0 Aluminum 5.5-6.5 Columbium t Ta 1.5-2.5 Silicon 0.50 max. Manganese 0.25 max. Copper 0.50 max. Sulphur 0.015 max. Iron 0.50 max. Nickel Remainder Specific gravity Density, lb/cu.in. Thermal coef. expansion/OF x 10-6 (70- 200OF) (70...
Abstract
View articletitled, ALLOY 713LC: High Temperature Nickel Alloy
View
PDF
for article titled, ALLOY 713LC: High Temperature Nickel Alloy
ALLOY 713LC is a nickel-base alloy possessing high stress-rupture strength up to 1700 F combined with excellent resistance to thermal fatigue. It is recommended for turbine wheels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-118. Producer or source: Austenal Microcast Division, Howmet Corporation.
Journal Articles
Alloy Digest (2019) 68 (8): SA-850.
Published: 01 August 2019
... 0.06 Titanium 0.05 Zirconium 0.15 Chromium 1.50 Copper 0.50 Nickel 2.00 Molybdenum 0.70 Boron 0.0050 Iron bal CEV max. acc. EN 10025-6 50 mm ( 2.0 in.) 0.47 > 50 120 mm (> 2.0 4.7 in.) 0.70 CEV standard value 50 mm ( 2.0 in.) 0.46 > 50 120 mm (> 2.0 4.7 in.) 0.46 CET 50 mm ( 2.0...
Abstract
View articletitled, ALDUR 500Q, QL, QL1: Structural Steel
View
PDF
for article titled, ALDUR 500Q, QL, QL1: Structural Steel
Aldur 500 steels (minimum yield strength of 500 MPa, or 73 ksi, for thicknesses up to 50 mm, or 2 in.) are a part family of water-quenched, high-strength, fine-grained steels that have excellent toughness at low temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low temperature performance. Filing Code: SA-850. Producer or source: Voestalpine Grobblech GmbH.
Journal Articles
Alloy Digest (2019) 68 (9): SA-851.
Published: 01 September 2019
... is a trademark of Voestalpine Grobblech GmbH Chemical Composition, wt.% (Typical, maximum) The steel is grain refined. Carbon 0.20 Silicon 0.80 Manganese 1.70 Phosphorus 0.020 Sulfur 0.010 Aluminum (total) 0.018 Nitrogen 0.015 Vanadium 0.12 Niobium 0.06 Titanium 0.05 Zirconium 0.15 Chromium 1.50 Copper 0.50...
Abstract
View articletitled, ALDUR 550Q, QL, QL1: Structural Steel
View
PDF
for article titled, ALDUR 550Q, QL, QL1: Structural Steel
Aldur 550 steels (minimum yield strength of 550 MPa, or 80 ksi, for thicknesses up to 50 mm, or 2 in.) are a part family of water-quenched, high-strength, fine-grained steels that have excellent toughness at low temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low temperature performance. Filing Code: SA-851. Producer or source: Voestalpine Grobblech GmbH.
Journal Articles
Alloy Digest (2020) 69 (11): Ti-172.
Published: 01 November 2020
... beta alloys because it is easier to melt and process, exhibiting low segregation, good workability, and good heat-treating properties. Chemical Composition Element Carbon Oxygen Nitrogen Hydrogen Iron Aluminum Vanadium Palladium Molybdenum Chromium Zirconium Yttrium Others, each Others, total Titanium...
Abstract
View articletitled, CARTECH Ti-3Al-8V-6Cr-4Mo-4Zr (BETA C): Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
View
PDF
for article titled, CARTECH Ti-3Al-8V-6Cr-4Mo-4Zr (BETA C): Ti-3Al-8V-6Cr-4Mo-4Zr Alloy
CarTech Ti-3Al-8V-6Cr-4Mo-4Zr, also known as Ti-3-8-6-4-4 and Beta C, is a metastable beta alloy used in the solution heat treated or solution heat treated and aged condition. It is appropriate for applications where very high strength, minimum weight, and corrosion resistance are important. Ti-3Al-8V-6Cr-4Mo-4Zr has gained in popularity among beta alloys because it is easier to melt and process, exhibiting low segregation, good workability, and good heat-treating properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-172. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... Inc. Chemical Composition, wt%: Element Composition, wt.% Hafnium 10.0 Titanium 0.7 1.3 Zirconium 0.7 Tantalum 0.5 Tungsten 0.5 Element Guaranteed impurity, ppm Carbon <150 Hydrogen <10 Iron <50 Copper <40 Chromium <20 Manganese <20 Nickel <20 Vanadium <20 Tin <10 Oxygen <225 Nitrogen <150 Silicon <50...
Abstract
View articletitled, C-103: Niobium Alloy
View
PDF
for article titled, C-103: Niobium Alloy
Alloy C-103 is a niobium alloy with a high strength/density ratio for elevated temperature applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: CB-25. Producer or source: ATI Wah Chang, Allegheny Technologies.