Journal Articles
Alloy Digest (2023) 72 (5): Ti-192.
Published: 01 May 2023
... Aubert & Duval TA6V ELI (UNS R56401) is an alpha-beta, titanium-aluminum-vanadium alloy that is normally used in the annealed condition. It is a purer version of Aubert & Duval TA6V, with a lower oxygen and iron content. Aubert & Duval TA6V ELI is especially popular due to its...
Journal Articles
Alloy Digest (2002) 51 (7): Ti-129.
Published: 01 July 2002
... tensile properties Titanium-Aluminum-Vanadium ELI workability thermal properties Chemical Composition, wt (Type Analysis) Carbon 0.080 max Aluminum 5.5 6.5 Nitrogen 0.050 max Oxygen 0.13 max Vanadium 3.5 4.5 Iron 0.25 max Hydrogen 0.013 max Other, total 0.40 max Other, each 0.1 max Hydrogen 0.0125...
Journal Articles
Alloy Digest (2005) 54 (11): Ti-137.
Published: 01 November 2005
... properties UNS R56401 Chemical Composition, wt Nitrogen 0.05 max Carbon 0.08 max Hydrogen 0.0125 max Iron 0.25 max Oxygen 0.13 max Aluminum 5.50 6.75 Vanadium 3.50 4.50 Titanium bal Other elements, total 0.30 max Other elements, each 0.10 max Physical Properties: Density, kg/m3 (lb/in.3 ) 4470 (0.160...
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... (Typical) Aluminum 5.5 6.5 Niobium 6.5 7.5 Tantalum 0.50 max Iron 0.25 max Oxygen 0.20 max Carbon 0.08 max Nitrogen 0.05 max Hydrogen 0.009 max Titanium bal Physical Properties: Beta transus temperature, °C (°F) 1010 ± 15 (1850 ± 27) Density, kg/m3 (lb/in.3) 4520 (0.163) Melting range, °C (°F) 1538 1649...
Journal Articles
Alloy Digest (2021) 70 (5): Ti-178.
Published: 01 May 2021
... (32 °F) Oxygen 0.03 0.08 6.6 Aluminum (3.8)(b) Vanadium 0.003 0.012(c) Titanium 580 0.10 0.25 (0.140) 0.10 0.13 1.68 (1008) 6 5.5 6.50 1.00005(c) 4 3.5 4.5 Typical values for wrought Timetal 6-4, 6-4 ELI & 6-4-.1Ru. (a) ±14 °C (±25 °F). (b) For mill annealed condition. (c) At 1.59 kA/m (20 Oe) bal...
Journal Articles
Alloy Digest (1988) 37 (12): Ti-89.
Published: 01 December 1988
... is a registered trademark of the RMI Company. **ELI = Extra Low Interstitials. Composition: Carbon Iron Aluminum Vanadium Nitrogen Oxygen Hydrogen Sheet Bar Billet Titanium 0.08 max. 0.25 max. 5.50-6.50 3.50-4.50 0.05 max. 0. I3 max. 0.150 max. 0.125 max. 0.100 max. Remainder Physical Constants: Density, lb/cu...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... A240 limits, maximum) Aluminum 5.50 6.75 Vanadium 3.50 4.50 Carbon 0.08 Oxygen 0.13 Nitrogen 0.05 Hydrogen 0.013 Iron 0.25 Other elements Each 0.10 Total 0.30 Titanium bal Physical Properties: Melting range, °C (°F) 1538 1649 (2800 3000) Density, kg/m3 (lb/in.3) 4430 (0.160) Beta transus temperature...
Journal Articles
Alloy Digest (2014) 63 (9): Ti-157.
Published: 01 September 2014
.... It is an extra low interstitial alloy with a high purity, which confers improved ductility and fracture toughness. SANDVIK BIOLINE Ti6Al4V ELI (Titanium Alloy) SANDVIK BIOLINE Ti6Al4V ELI Chemical Composition, wt (Nominal, maximum) Aluminum 5.5 6.50 Vanadium 3.5 4.5 Iron 0.25 Carbon 0.08 Hydrogen 0.12 Oxygen...
Journal Articles
Alloy Digest (2007) 56 (11): Ti-143.
Published: 01 November 2007
... workability thermal properties Chemical Composition, wt 6-4 6-4 ELI 6-4-.1Ru Aluminum 5.50 6.75 5.5 6.5 5.5 6.5 Vanadium 3.5 4.5 3.5 4.5 3.5 4.5 Iron 0.40 max 0.25 max 0.25 max Oxygen 0.20 max 0.13 max 0.13 max Carbon 0.08 max 0.08 max 0.08 max Nitrogen 0.05 max 0.03 max 0.03 max Hydrogen 0.015 max 0.0125...
Journal Articles
Alloy Digest (1998) 47 (9): Ti-114.
Published: 01 September 1998
... products with the most notable being bicycle tubing. Table 3 AWS Composition for Welding Rods and Electrodes Composition, wt.% Elemeot Aluminum ERTi3Ab2.9 - ERTi 3Al-2.9 ELI(a) 2.5-3.5 2.5-3.5 Vanadium 2.0-3.0 2.b3.0 Nitrogen 0.02 Ina 0.012 max Carbon 0.05 max 0.04 max oxygen 0.12 max 0.10 max Iron 025max...
Journal Articles
Alloy Digest (2004) 53 (7): Ti-133.
Published: 01 July 2004
... workability thermal properties Chemical Composition, wt (Typical) Aluminum 4 Vanadium 2.5 Iron 1.5 Oxygen 0.250 Titanium bal Ruthenium can be added for better corrosion resistance. Physical Properties: Density, kg/m3 (lb/in.3 ) 4490 (0.162) Melting range, °C (°F) 1600 1650 (2912 3002) Mechanical...
Journal Articles
Alloy Digest (2002) 51 (8): Ti-60.
Published: 01 August 2002
... Carpenter Titanium-Aluminum-Vanadium chemical composition compressive strength corrosion-resistant alloys elasticity fatigue properties fracture toughness heat treatability high-temperature alloys joinability machinability physical properties shear strength tensile properties workability...
Journal Articles
Alloy Digest (2021) 70 (3): Ti-176.
Published: 01 March 2021
... can provide considerable cost savings by being significantly easier to process and machine. Chemical Composition Composition, wt%(a) Property Unit At Value 3.5 4.3 Density Element Thermal conductivity kg/m3 24 °C 4530 Vanadium 0.55 1.15 Thermal diffusivity (lb/in.3) (75 °F) (0.164) Aluminum 0.20 0.30...