... TIMKEN TBS-9 is a high-carbon, chromium-molybdenum ball-bearing steel that combines high hardenability and low cost. It was designed with metallurgical properties virtually equivalent to those of AISI 52100. TBS-9 is less expensive than the 52100 grade because annealing is simplified. It is...
Journal Articles
Alloy Digest (1984) 33 (6): TS-423.
Published: 01 June 1984
... toughness. Such applications include punches, dies and cold-forming rolls. *NDS is a registered trademark of Latrobe Steel Company. a subsidiary of The Timken Company. Composltion: Typical Analysis Carbon 0.75 Manganese 0.30 Silicon 0.25 Chromium 1.00 Nickel 1.70 Iron Remainder Physical Constants: Density...