Skip Nav Destination
Close Modal
Search Results for
TiCode-12
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for TiCode-12
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1979) 28 (2): Ti-71.
Published: 01 February 1979
... TiCode-12 is a titanium-base alloy developed for corrosion-resisting applications. It contains nominally 0.8% nickel and 0.3% molybdenum; these additions affect corrosion resistance profoundly. They also provide an added benefit by significantly strengthening the titanium through the introduction...
Abstract
View articletitled, <span class="search-highlight">TiCode</span>-<span class="search-highlight">12</span>: Corrosion Resistant Titanium Alloy
View
PDF
for article titled, <span class="search-highlight">TiCode</span>-<span class="search-highlight">12</span>: Corrosion Resistant Titanium Alloy
TiCode-12 is a titanium-base alloy developed for corrosion-resisting applications. It contains nominally 0.8% nickel and 0.3% molybdenum; these additions affect corrosion resistance profoundly. They also provide an added benefit by significantly strengthening the titanium through the introduction of a small amount of beta phase into the structure and through solution effects. TiCode-12 has many applications in the process industries where its excellent corrosion resistance is needed. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-71. Producer or source: Titanium Metals Corporation of America.