1-20 of 47

Search Results for Ti-6Al-4V

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2020) 69 (10): Ti-171.
Published: 01 October 2020
... ATI 6-4 is an alpha-beta, Ti-6Al-4V alloy that is used in the annealed condition, or in the solution heat treated and aged condition. This high-strength alloy can be used at cryogenic temperatures up to about 425 °C (800 °F). Ti-6Al-4V is the most widely used titanium alloy. This datasheet...
Journal Articles
Alloy Digest (2023) 72 (4): Ti-191.
Published: 01 April 2023
... properties workability UNS R56400 AUBERT & DUVAL TA6V (Wrought Ti-6Al-4V Alloy) Filing Code: Ti-191 Titanium :: April 2023 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: [email protected] Published by ASM International® :: Data shown are typical...
Journal Articles
Alloy Digest (2023) 72 (5): Ti-192.
Published: 01 May 2023
... treatability joinability machinability physical properties tensile properties thermal properties workability UNS R54601 AUBERT & DUVAL TA6V ELI (Wrought Ti-6Al-4V Alloy) Filing Code: Ti-192 Titanium :: May 2023 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org...
Journal Articles
Alloy Digest (2021) 70 (1): Ti-174.
Published: 01 January 2021
... properties corrosion-resistant alloys heat treatability machinability joinability UNS R56406 ARCAM Ti6Al4V (Ti-6Al-4V Alloy) Filing Code: Ti-174 Titanium :: January 2021 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: [email protected] Published...
Journal Articles
Alloy Digest (2021) 70 (5): Ti-178.
Published: 01 May 2021
... Company) Copyright © ASM International® 2021 2021 ASM International Arcam Ti6Al4V ELI (Grade 23) chemical composition physical properties microstructure hardness elasticity tensile properties machinability joinability thermal properties UNS R56401 ARCAM Ti6Al4V ELI (Ti-6Al-4V ELI...
Journal Articles
Alloy Digest (1992) 41 (9): Ti-66.
Published: 01 September 1992
... heat treatability high-temperature alloys joinability low-temperature alloys machinability physical properties tensile properties Ti-6Al-4V workability Filing Code: n-66 Titanium Alloy Revised SEPT. 1992 - DIGEST- JUNE 1972 DATA ON WORLD WIDE METALS AND ALLOYS gzi2=az1m= -Yi!s&zP - P...
Journal Articles
Alloy Digest (2002) 51 (7): Ti-129.
Published: 01 July 2002
... Carpenter titanium alloy Ti 6Al-4V ELI is a high-purity (extra-low-interstitial) version of Ti 6Al-4V (see Alloy Digest Ti-60, August 2002). The alloy is alpha plus beta and has good biocompatibility. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (2002) 51 (8): Ti-60.
Published: 01 August 2002
... high strength for a lightweight material. Specific strength is strength/density and provides a means to compare materials. See Table 2 for comparison. Fatigue Limits. High-cycle fatigue limits for Ti 6Al-4V are greatly influ- enced by both microstructure and surface conditions. Generalized axial...
Journal Articles
Alloy Digest (2023) 72 (2): Ti-189.
Published: 01 February 2023
... ATI 6-6-2 (UNS R56620) is a highly beta-stabilized, two-phase, alpha-beta titanium alloy which is a modification of the Ti-6Al- 4V system. Because of the higher beta stabilizing elements (additional vanadium plus iron and copper), this alloy has a higher strength potential than ATI Ti-6Al-4V alloy...
Journal Articles
Alloy Digest (2002) 51 (1): Ti-125.
Published: 01 January 2002
... Ti 6Al-4V-0.1Ru alloy is an extra-low interstitial alloy version of Ti-6Al-4V offering improved fracture toughness in air and better corrosion resistance to crude oil with chlorides. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2004) 53 (7): Ti-133.
Published: 01 July 2004
... ATI 425 was originally developed for hot-rolled armor plate to provide ballistic protection comparable to Ti-6Al-4V and has been evaluated against a variety of projectile threats for use as armor. While processing the alloy for armor plate applications, it was observed that the material exhibited...
Journal Articles
Alloy Digest (2001) 50 (12): Ti-123.
Published: 01 December 2001
... TIMETAL 367 is a Ti-6Al-7Nb medium-strength alpha-beta alloy for surgical implants. The alloy is analogous to TIMETAL 367 6-4 (revised as Ti-6Al-4V, Alloy Digest Ti-66, September 1992), but with niobium as the more biocompatible alloying element. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... Allvac Titanium Alloy 6Al-7Nb uses niobium to stabilize the beta phase. It is very similar to Ti-6Al-4V and is widely used in medical and surgical device applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... ATI 6-4 ELI, also known as Grade 23, is a higher purity grade of ATI Ti-6Al-4V for use in surgical and medical applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (2021) 70 (3): Ti-176.
Published: 01 March 2021
... Timetal 407 (Ti407) is a wrought, heat-treatable, alpha–beta, Ti-V-Al-Si-Fe alloy that excels in applications requiring resistance to impact, explosive blast, and/or other forms of shock loading. Its properties are generally similar to those of Ti-6Al-4V or Ti-3Al- 2.5V; however, in comparison...
Journal Articles
Alloy Digest (2020) 69 (12): Ti-173.
Published: 01 December 2020
... °C, or 750 °F). Ti-6Al-4V is the most widely used titanium alloy, accounting for more than 50% of the total titanium used. The aerospace industry accounts for more than 80% of this usage. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2023) 72 (8): Ti-195.
Published: 01 August 2023
... Aubert & Duval Ti17 (UNS R58650) is a “beta-rich” alpha-beta titanium-aluminum-molybdenum-chromium-zirconium-tin alloy. This alloy has higher tensile and creep strengths than Ti-6Al-4V. While its hardenability is similar to that of other beta alloys, Aubert & Duval Ti17 has a lower density...
Journal Articles
Alloy Digest (2020) 69 (5): Ti-166.
Published: 01 May 2020
... ATI 3-2.5 is a Titanium-3Aluminum-2.5Vanadium alloy that has higher strength than unalloyed titanium and is much more amenable to cold working than Ti-6Al-4V. This near-alpha, alpha-beta alloy is generally used in the annealed or cold-worked and stress-relieved conditions. This datasheet provides...
Journal Articles
Alloy Digest (1997) 46 (12): Ti-111.
Published: 01 December 1997
... 3M TITANIUM MATRIX COMPOSITES are produced by electron-beam evaporation to apply Ti-6Al-4V coating to high-strength, high-modulus silicon carbon fibers. The resulting composite has increased strength and stiffness over monolithic titanium/titanium alloy parts. This datasheet provides information...
Journal Articles
Alloy Digest (2008) 57 (8): Ti-146.
Published: 01 August 2008
... Timetal 54M has better machinability than TI-6Al-4V with comparable properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating...