Alloy Digest (2021) 70 (12): Ti-185.
Published: 01 December 2021
... Smiths Ti-6Al-2Sn-4Zr-2Mo-Si is a near-alpha titanium alloy that was developed for use at elevated temperatures. It exhibits high strength and toughness, excellent creep resistance, and high temperature stability at temperatures up 550 °C (1020 °F). This datasheet provides information...
Journal Articles
Alloy Digest (1967) 16 (8): Ti-52.
Published: 01 August 1967
... Ti-6Al-2Sn-4Zr-2Mo is a super-alpha titanium alloy providing an excellent combination of creep strength, tensile strength, toughness and stability to 1050 F. It is recommended for airframe and gas turbine engine requirements. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2020) 69 (8): Ti-169.
Published: 01 August 2020
...-6Al-2Sn-4Zr-2Mo Alloy) Filing Code: Ti-169 Titanium :: August 2020 :: :: :: ::Materials Park, Ohio 44073-0002 440.338.5151 Fax 440.338.4634 www.asminternational.org MemberServiceCenter@asminternational.org ::Published by ASM International® Data shown are typical, not to be used for specification...
Journal Articles
Alloy Digest (1981) 30 (8): Ti-83.
Published: 01 August 1981
... 1996 1996 ASM International bend strength chemical composition corrosion-resistant alloys creep strength elasticity heat treatability jet engines components joinability machinability physical properties RMI 6Al-2Sn-4Zr-2Mo tensile strength workability All OY Filing Code: Ti-83 RMI...
Journal Articles
Alloy Digest (1972) 21 (4): Ti-64.
Published: 01 April 1972
... International chemical composition corrosion-resistant alloys elasticity fatigue properties heat treatability high-temperature alloys joinability machinability physical properties tensile properties Ti-6Al-2Sn-4Zr-6Mo workability All 08 APRIL 1972 DIGESTfl - DATA ON WORLD WIDE METALS...