Alloy Digest (1966) 15 (11): Ti-48.
Published: 01 November 1966
... Ti-679 is a titanium high temperature alloy having an excellent combination of short-time strength, creep strength and stability to 900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (2002) 51 (2): Ti-126.
Published: 01 February 2002
... TIMETAL 679 is a Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si alloy with three phases at room temperature. It has high strength with creep resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep and fatigue. It also...
Journal Articles
Alloy Digest (2002) 51 (4): Cu-679.
Published: 01 April 2002
... brass alloys. Alloy 58D has total nonmagnetic quali- ties. The free-machining brasses are listed in order of increasing SWISSMETAL® SM117N, SM118N, SM121N (BOILLAT 58T, 58A, 58F) Filing Code: Cu-679 Copper April 2002 SWISSMETAL® SM117N, SM118N, SM121N (BOILLAT 58T, 58A, 58F) (Free-Machining Brass...