1-6 of 6 Search Results for

Ti-50A

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1992) 41 (8): Ti-100.
Published: 01 August 1992
... TIMET GRADES Ti-35A, Ti-50A, Ti-65A, Ti-75A, Ti-100A unalloyed titanium offer good ductility and cold formability, good to excellent weldability, and good to excellent corrosion resistance in neutral to oxidizing environments, including chlorides. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1972) 21 (6): Ti-65.
Published: 01 June 1972
... Ti-35A and Ti-50A are commercially pure titanium grades with guaranteed minimum tensile strengths of 35000 psi and 50,000 psi, respectively. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (1979) 28 (2): Ti-71.
Published: 01 February 1979
... = Resisted (samples showed no evidence of corrosion). Table 5 - RESISTANCE TO BOILING l21Ool-)705; AMMONIUM HYDROXIDE Alloy Corrosion* Ti-5OA Nil TiCode- 2 Nil TI-Pd Nil *Too low to measure. 500-hr exposure. Tabla 6 - RESISTANCE TO NITRIC ACID VAPORS Alloy Corrosion Rate, mils/year* Ti-50A 2.0 TiCode- 2 0.8...
Journal Articles
Alloy Digest (2001) 50 (9): Ti-120.
Published: 01 September 2001
... procedures, although the latter methods can be used only if the material is protected from atmospheric contamination. This grade is used in airframe and chemical process applications. TIMETAL® 50A (Commercially Pure Titanium) Filing Code: Ti-120 Titanium September 2001 TIMETAL® 50A Chemical Composition, wt...
Journal Articles
Alloy Digest (2010) 59 (5): Ti-147.
Published: 01 May 2010
..., elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TI-147. Producer or source: Timet. Producer or Source: Timet Copyright © ASM International® 2010 2010 ASM International chemical...
Journal Articles
Alloy Digest (1998) 47 (9): Ti-114.
Published: 01 September 1998
... TIMETAL 3-2.5 (Ti-3%Al-2.5%V) alloy is cold formable and weldable. This alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications, such as pressure vessels and piping, also utilize this alloy. The alloy is available with palladium stabilization...