Alloy Digest (1994) 43 (2): TS-523.
Published: 01 February 1994
... THYSSEN P20 SUPER is a modified P20 with higher carbon and nickel to improve impact strength and temper resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating, machining, and surface treatment. Filing Code...
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
...; Thyroplast 2798; Thyssen P20 Super mold materials, together with Thyrotherm 2344 EiFS Supra as a die casting die. De- signed as a holder material, it can also be used for non- demanding plastic molds which require no better than a #2 ftish. Applications: This holder material is primarily for both plastic...